cold formed steel presentation

16
William Hutton

Upload: whutton1

Post on 20-Jan-2015

717 views

Category:

Documents


7 download

DESCRIPTION

A presentation I have given at the University of Southern Queensland on the design of Cold-Formed Steel Battens

TRANSCRIPT

Page 1: Cold Formed Steel Presentation

William Hutton

Page 2: Cold Formed Steel Presentation

• Knowledge Gap• Specification B1.2 of the BCA• Testing and the Analysis of this Testing• The Effective Width Method• The Direct Strength Method• Results • Conclusion

Page 3: Cold Formed Steel Presentation

1.Little Research conducted on effect and value of lateral and torsional restraint on hat sections.

2.Torsional restraint of corrugated roof cladding profiles.

3.DSM on the hat sections, to allow them to become classified as pre-qualified sections.

Page 4: Cold Formed Steel Presentation

• States that ALL metal roofing systems, specifically metal roof cladding, its connections and its immediate supporting members, used in cyclonic regions shall be tested using Low-High-Low (LHL) test regime.

Sequence No. of Cycles Load

A 4500 0 to 0.45Pt

B 600 0 to 0.6 Pt

C 80 0 to 0.8 Pt

D 1 0 to 1.0 Pt

E 80 0 to 0.8 Pt

F 600 0 to 0.6 Pt

G 4500 0 to 0.45 Pt

Page 5: Cold Formed Steel Presentation

• Batten Webo Upward dooming of the

screw holeo 2 to 3 cracks forming

perpendicular to the hole

• Batten Feeto Screw tears through batten

feet, commencing at the feet-web junction

Page 6: Cold Formed Steel Presentation

Batten Type

No. of Tests

Factor of Variability, kt

Applied Load, Pt

Ultimate Limit State Strength

40x0.75 4 1.50 5.37 3.58

64x0.75 1 1.79 4.90 2.73

64x1.00 1 1.79 5.21 2.91

Page 7: Cold Formed Steel Presentation
Page 8: Cold Formed Steel Presentation
Page 9: Cold Formed Steel Presentation

• Applies the Finite Strip Method to the given profile.

• Provides Load factors for each buckling mode.• Provides the yielding moment, My• Provides the yielding compressive force, Py• These values are then used to calculate the

Local and Elastic Buckling stress

Page 10: Cold Formed Steel Presentation

Local BucklingLoad Factor = 0.71Half-Wavelength=1.6” Distortional Buckling

Load Factor = 6.39Half-Wavelength=21.0”

Page 11: Cold Formed Steel Presentation

• Utilises the elastic buckling stress calculated from the output of CUFSM and Gross Section Properties of the profile.

• Analyses the batten for a given span and allows the the effects of lateral restraint, torsional restraint and load height on the batten to be considered.

• Adopted Kry=1000kN/rad and krx=0kN/rad.

Page 12: Cold Formed Steel Presentation
Page 13: Cold Formed Steel Presentation

• Test Batten Connection to LHL regime• Analysis results as per AS/NZS1170.0• Calculate gross section properties.• Calculate elastic buckling stresses in CUFSM• Calculate load-span capacity using PURLIN.• Combine testing and numerical analysis to

determine the load-span capacity using Spread Sheet program and develop the load-span tables.

Page 14: Cold Formed Steel Presentation

Load-Span Capacity table for 40x0.75mm Batten

Span 2 Batten Screws 4 Batten Screws

w*u,uplift w*u,down w*u,uplift w*u,down

600 4.692 4.692 Cladding Connection Fatigue Strength

4.692 4.692 Cladding Connection Fatigue Strength

900 3.616 3.616 Batten Feet Fatigue Strength

4.692 4.692 Cladding Connection Fatigue Strength

1200 2.712 2.712 Batten Feet Fatigue Strength

3.187 3.526 Uplift: DSM Analysis. Downthrust: Connection Fatigue Strength

1500 2.030 2.170 Uplift: DSM Analysis,Downthrust: connection Fatigue Strength

2.030 2.351 Uplift: DSM Analysis. Downthrust: Connection Fatigue Strength

Page 15: Cold Formed Steel Presentation

• The DSM provides better results than the EWM.

• The design procedure allows for quick efficient batten design.

• For short spans, the connection capacity governs thus LHL testing critical

Page 16: Cold Formed Steel Presentation

Thank You