delayed coking (saswiny presentation)
TRANSCRIPT
![Page 1: Delayed Coking (Saswiny Presentation)](https://reader035.vdocuments.net/reader035/viewer/2022062323/5695cfd81a28ab9b028fc256/html5/thumbnails/1.jpg)
![Page 2: Delayed Coking (Saswiny Presentation)](https://reader035.vdocuments.net/reader035/viewer/2022062323/5695cfd81a28ab9b028fc256/html5/thumbnails/2.jpg)
![Page 3: Delayed Coking (Saswiny Presentation)](https://reader035.vdocuments.net/reader035/viewer/2022062323/5695cfd81a28ab9b028fc256/html5/thumbnails/3.jpg)
![Page 4: Delayed Coking (Saswiny Presentation)](https://reader035.vdocuments.net/reader035/viewer/2022062323/5695cfd81a28ab9b028fc256/html5/thumbnails/4.jpg)
![Page 5: Delayed Coking (Saswiny Presentation)](https://reader035.vdocuments.net/reader035/viewer/2022062323/5695cfd81a28ab9b028fc256/html5/thumbnails/5.jpg)
![Page 6: Delayed Coking (Saswiny Presentation)](https://reader035.vdocuments.net/reader035/viewer/2022062323/5695cfd81a28ab9b028fc256/html5/thumbnails/6.jpg)
![Page 7: Delayed Coking (Saswiny Presentation)](https://reader035.vdocuments.net/reader035/viewer/2022062323/5695cfd81a28ab9b028fc256/html5/thumbnails/7.jpg)
Green Coke
Directly produced with no further processing
Primarily used for fuel
Uncalcined sponge coke typically 14,000 Btu/lb heating value
Crushed & drained of free water
Calcined Coke
Green coke heated to finish carbonizing coke & reduce volatile matter to very low levels
Done in rotary kiln or rotary hearth
Heated 1800-2400°F
Does not remove metals