“Thanks for the pictures. Any other pictures that you have would be great as I will use them to put in the newspaper and also present them to our school board members. I am very impressed with the job you guys did and the professionalism of the workers. You have my full recommendation for any job you are seeking”.

Micky LivelySuperintendent, Mangum Schools

Page 2: Mangum School

EXISTING ROOFGranulated Modified Bitumen – 40,000 sq.ft.

Page 3: Mangum School

Granulated Modified Bitumen

Checking depth of alligator cracks in ponding areas

Page 4: Mangum School

SURFACE PREPARATIONHigh Pressure Power Wash with Bio-degradable Cleaner

NEOGARD8500 Bio-Degradable Cleaner

Page 5: Mangum School

Bad areas & protrusions detailed with Polyurethane Foam

“Reddish” color is 7780/7781 Primer1/3 gal/100 sq.ft.

Page 6: Mangum School

7419 HB Urethane Base Coat350 psi tensile strength500% Elongation1.5 gal/100 sq.ft. – 18 dry mils

Page 7: Mangum School

After Base Coat is Applied to Entire Roof2nd Coat of 7419 HB is Applied to the Seams

Page 8: Mangum School

70613 Urethane Topcoat2,500 psi tensile strength450% Elongation1.5 gal/100 sq.ft. – 18 dry mils

Page 9: Mangum School

#11 Roofing Granules Applied Over Wet Topcoat

Total System Elastomeric Coating Thickness to Average 36 Dry Mils for this Project

Page 10: Mangum School

10 & 15 Year Warranty Requirements10-Year Warranty:

3. Clean roof with high pressure power wash & 8500 Biodegradable cleaner

4. Primer: 7780/7781 epoxy primer at the rate of 1/3 gal/100 sq.ft.

5. Base Coat: 7419 HB urethane at minimum rate of 1.5 gal/100 sq.ft. – 18 dry mils

6. Topcoat: 70613 urethane at a minimum rate of 1.5 gal/100 sq.ft. – 18 dry mils

Total system elastomeric coating thickness to average 36 dry mils

15-Year Warranty:

• Clean roof with high pressure power wash & 8500 Biodegradable cleaner

• Primer: 7780/7781 epoxy primer at the rate of 1/3 gal/100 sq.ft.

• Base Coat: 7419 HB urethane at a minimum rate of 3 gal/100 sq.ft. – 36 dry mils

• Topcoat: 70613 urethane at a minimum rate of 1.5 gal/100 sq.ft. – 18 dry mils

Total system elastomeric coating thickness to average 54 dry mils

Page 11: Mangum School

CURT CARPENTER C&G COATINGS

Your NEOGARD® Representative

Thank you for your time. Please feel free to contact me for an estimate or more information on the NEOGARD® product

and application that’s right for you.

8228 Marshall Dr.Lenexa, KS 66214

913-438-2412 – office913-634-2588 – cell913-492-4362 – fax

[email protected]


Top Related