    Knife Line AttackCompiled and edited by

    Nasrizal Mohd Rashdi

    Senior LecturerFabrication & Joining Section

    Universiti Kuala Lumpur

  • 7/22/2019 Knife Line Attack Welding Defect

    2/15

    Knife Line Attack

    Occur in stabilized austenitic stainless

    steel such as 321 & 347.

    It also inter-granular corrosion but not

    same as weld decay.

    Also cause by precipitation of Chromium

    carbide at grain boundary.

  • 7/22/2019 Knife Line Attack Welding Defect

    3/15

    Differs from weld decay

    Occurs in narrow band in the area

    immediately adjacent to weld metal.

    Occurs in stabilized SS

  • 7/22/2019 Knife Line Attack Welding Defect

    4/15

  • 7/22/2019 Knife Line Attack Welding Defect

    5/15

  • 7/22/2019 Knife Line Attack Welding Defect

    6/15

  • 7/22/2019 Knife Line Attack Welding Defect

    7/15

    Mechanism

    The area corresponding to thermal cycle

    1 is very close to the fusion boundary

    Therefore is subjected to both a very high

    peak temperature and a very rapid cooling

    rate during welding.

    This peak temperature is above the solvus

    temperature of titanium carbide, so it will

    dissolves in this area.

  • 7/22/2019 Knife Line Attack Welding Defect

    8/15

    Mechanism

    Because of the rapid cooling rate through its

    precipitation temperature range, titanium carbide

    does not re-precipitate during cooling

    Thus leaving abundant free carbon atoms in thisarea.

    When the weld is reheated in the Cr carbide

    precipitation range (for stress-relief or in

    multiple-pass welding), Ti carbide does not form

    appreciably since the temperature level is not

    high enough.

  • 7/22/2019 Knife Line Attack Welding Defect

    9/15

    Consequently, Cr carbide precipitates at

    grain boundaries, and this area becomes

    susceptible to intergranular corrosion

    attack.

  • 7/22/2019 Knife Line Attack Welding Defect

    10/15

    Because of the high temperate gradient

    near the fusion boundary and the high Ti

    carbide dissolution temperature, the region

    in which Ti carbide dissolves duringwelding is very narrow

  • 7/22/2019 Knife Line Attack Welding Defect

    11/15

    As a result, subsequent intergranular

    corrosion attack occurs in a very narrow

    strip immediately adjacent to the fusion

    boundary, and thus the name knife-lineattack. Figure 18.15 shows the

    transmission electron

  • 7/22/2019 Knife Line Attack Welding Defect

    12/15

  • 7/22/2019 Knife Line Attack Welding Defect

    13/15

    Prevention methods

    Addition of rare earth metal ( La + Ce).

    It reduce the rate of intergranular corrosion.(see fig. 18-18).

    It no adverse effects on mechanicalproperties.

    Post weld heat treatment.

    Heat to 1000OC to 1100OC, to dissolving thechromium carbide and than rapid quenching.

    Use low carbon grade.

  • 7/22/2019 Knife Line Attack Welding Defect

    14/15

  • 7/22/2019 Knife Line Attack Welding Defect

    15/15

    Question

    State the area are possibility to knife line

    attack

    second pass

    FirstPass