WELDING INSPECTION

Welding inspection is used to verify that welding has been performed in accordance with the appropriate welding procedure and that the result has produced a compliant weld

Welding inspection techniques include visual inspection, non-destructive and destructive testing as well as audits of the process

A defect is a condition of the weld that is out-with the boundaries of acceptability in relation to the particular standard

Page 3: Welding Defects

3

Page 4: Welding Defects

4

Page 5: Welding Defects

5

Page 6: Welding Defects

6

Page 7: Welding Defects

7

Page 8: Welding Defects

8

Page 9: Welding Defects

9

Page 10: Welding Defects

10

Page 11: Welding Defects

11

Page 12: Welding Defects

12

Page 13: Welding Defects

13

Linear Misalignment

Offset or Mismatch

High-low

Manual Metal

Arc Welding MMA

Page 14: Welding Defects

14

Offset or Mismatch

with lack of Root

Fusion

Manual Metal

Arc Welding MMA

Page 15: Welding Defects

15

Cap concavity or insufficient fill

Manual Metal

Arc Welding MMA

Page 16: Welding Defects

16

Excessive root penetration

Manual Metal

Arc Welding MMA

Page 17: Welding Defects

17

External Undercut Manual Metal

Arc Welding MMA

Page 18: Welding Defects

18

Root Undercut Manual Metal

Arc Welding MMA

Page 19: Welding Defects

19

Root Concavity (suck back)

Manual Metal

Arc Welding MMA

Page 20: Welding Defects

20

Root burn-through Manual Metal

Arc Welding MMA

Page 21: Welding Defects

21

Incomplete or lack of root penetration

Manual Metal

Arc Welding MMA

Page 22: Welding Defects

22

Inter-pass Slag Inclusions

Manual Metal

Arc Welding MMA

Page 23: Welding Defects

23

Elongated Slag lines (wagon tracks)

Manual Metal

Arc Welding MMA

Page 24: Welding Defects

24

Lack of side wall fusion

Tungsten Inert Gas Welding TIG

Page 25: Welding Defects

25

Inter-pass cold lap-lack of side wall fusion

Tungsten Inert Gas Welding TIG

Page 26: Welding Defects

26

Scattered Porosity

Manual metal arc welding MMA

Page 27: Welding Defects

27

Cluster Porosity Manual metal arc welding MMA

Page 28: Welding Defects

28

Root aligned porosity

Tungsten Inert Gas Welding TIG

Page 29: Welding Defects

29

Transverse cracks Tungsten Inert Gas Welding TIG

Page 30: Welding Defects

30

Longitudinal crack TIG/MMA

Page 31: Welding Defects

31

Longitudinal root crack

Manual metal arc welding MMA

Page 32: Welding Defects

32

Tungsten inclusions Tungsten Inert Gas Welding TIG