Welding Procedure
Specification’s
(WPS)Presented By John Lucas
Welding Engineer
UTI Corporation
![Page 2: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/2.jpg)
What Is Welding?
AWS defines welding as:
“ The art and science of joining metals by using the intrinsic adhesive and cohesive forces of attraction that exist within metals”.
Welding, Brazing, Soldering
Does not include mechanical fastening such as bolts, rivets, screws, etc.
![Page 3: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/3.jpg)
When Did Welding Begin?Pressure Welding of Noble Metals
Over 2,000 years ago
Forge WeldingBlacksmiths
Over 1,000 years ago
Modern Welding1880’s
![Page 4: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/4.jpg)
Interesting FactTemperature Of The Sun?
9,941°F
Temperature Of The Arc?
12,632°F
![Page 5: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/5.jpg)
WELDING PROCEDURES
• What Is a Welding Procedure?
• Why Have Welding Procedures?
• Who Should Have Welding Procedures?
• What Information Should Procedures Contain?
• How do we know If Our Procedures Are Good?
![Page 6: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/6.jpg)
What Is A Welding Procedure?
• A document that contains important variables on how to make the weld in question.
![Page 7: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/7.jpg)
![Page 8: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/8.jpg)
Why Have Welding Procedures?
• Required By Code
• Proves To Engineers & Regulators You Know What You Are Doing
• Helps To Produce Quality Welds
![Page 9: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/9.jpg)
Who Should Have Welding Procedures?
• Manufacturing• Automotive
• Heavy Equipment
• Pipeline Industry
• Construction
![Page 10: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/10.jpg)
What Information Should I Include?
![Page 11: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/11.jpg)
Important Information
• Governing Code• API, AWS, ASME, ISO
• Foreign Codes
![Page 12: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/12.jpg)
Important Information
• Material Parameters• Spec & Grade
• Wall Thickness
• Size (Diameter)
• Yield/Tensile Strength
• Metallurgical Concerns
![Page 13: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/13.jpg)
Important Information
• Welding Process• GMAW (MIG), GTAW (TIG), SMAW (STICK)
• Automated Or Not?
![Page 14: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/14.jpg)
Important Information• Process Parameters
• Volts, Amps, Travel Speed
• Travel Direction
• Polarity
• Wire Welding Transfer Mode• Globular, Spray, Short Circuit, Plasma
• Flux Core or Shielding Gas
• Number of Passes
• Number of Welders
• Electrodes
Size
Group Number = 1, 2, 3, etc.
AWS Specification = A5.1, A5.5, etc.
![Page 15: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/15.jpg)
Important Information• Pre/Post Weld Heat Treatment
• Temps
• Time
• Cooling Rates
• Heat Input
• Time Interval Between Passes
![Page 16: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/16.jpg)
Important Information
• Joint Design• Material Thickness
• Joint Type
• Bevel Angles
• Root Opening Dimension
• Backer Rods
• Etc.
![Page 17: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/17.jpg)
Important Information
• Filler Metals
E 6010E = Electrode
60 = Tensile Strength (60,000psi)
1 = All Position
0 = Type Of Coating & Polarity
Cellulose, Low Hydrogen, Potassium, etc.
![Page 18: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/18.jpg)
Important Information
• Cleanliness• Joint Cleaning
• Coating Removal
• How to Remove Coatings
• Joint Fit Up• Line Up Clamps
• Internal or External
![Page 19: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/19.jpg)
Procedure Qualification Record
• Lab Report• Parameters/Materials
• Info Made for Each Pass
• Ambient Conditions
![Page 20: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/20.jpg)
Procedure Qualification Record
Testing Reports
![Page 21: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/21.jpg)
Welder Qualification
• Three Welder Testing ProceduresAPI 1104
Field Welding
ASME Section 9
Fab Shop Welding
Part 192-Appendix C
Low Stress
12 Inch And Less Pipe
![Page 22: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/22.jpg)
Welder Qualification
• Initial Test• Initial Test = Destructive
• 6 Month Retest• Non Destructive
• Compressor Station & Components» Part 192.229
» Destructive Only
• If a Welder Performs a Procedure Qualification, Is The Welder Also Qualilfied?
![Page 23: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/23.jpg)
Weld Quality
![Page 24: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/24.jpg)
Weld Quality
• Lack of Fusion
![Page 25: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/25.jpg)
Weld Quality
• Lack of Penetration
![Page 26: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/26.jpg)
Weld Quality
• Porosity
![Page 27: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/27.jpg)
Weld Quality
• Under Cut
![Page 28: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/28.jpg)
Welding Safety
![Page 29: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/29.jpg)
• Eye Safety• Wear a Hood
• Skin Safety• Burns
» Wear Sun Screen - SPF 45
• White Wall Effect
![Page 30: Welding Procedure - Ohio Gas · PDF file•What Is a Welding Procedure? •Why Have Welding Procedures? ... •Three Welder Testing Procedures API 1104 Field Welding ASME Section 9](https://reader034.vdocuments.net/reader034/viewer/2022042508/5a78b8617f8b9a852c8f01ac/html5/thumbnails/30.jpg)
Conclusion
• Comments Or Questions?