White Fused Alumina White corundum is produced from alumina by melting in the electric arc furna ce. Color : white Mohs hardness: 9 Crystal shape :trigonal sy stem, Chemical component : Al2O3 > 99%, Little amount of Sio2, Fe2O3, Na2O. Main application: abrasive s, refractories, polishing, sandblasting purposes.

Upload: hx-abrasives

Post on 15-Apr-2017

148 views

Category:

Presentations & Public Speaking


0 download

TRANSCRIPT

Page 1: White Carborundum

White Fused Alumina

White corundum is produced from alumina by melting in the electric arc furnace.Color : whiteMohs hardness: 9Crystal shape :trigonal system, Chemical component :Al2O3 > 99%, Little amount of Sio2, Fe2O3, Na2O.

Main application: abrasives, refractories, polishing, sandblasting purp

oses.

Page 2: White Carborundum

Smelting

There are two ways of smelting method:Fixed FurnaceTilting Furnace

color Smelting time

Hardness

Fixed Furnace

white short good

Tilting Furnace

white but dark

long better

Page 3: White Carborundum

Tilting Furnace

Page 4: White Carborundum

Fixed Furnace

Page 5: White Carborundum

Manufacturing of grains

Grain size:

F standard F4-F220 P12-P220

Section sand: 0-1mm, 1-3mm,3-5mm, 5-8mm

Finer: 200#,325#

White corundum block → coarse crushing → ball mill or roller machine (the grain shape

depends on the manufacturing technique, the ball mill better than roller machine)→magnetic

separation →screening particle size (vibration sieve) → sampling test particle size distribution

→bagging finished products

Page 6: White Carborundum

• Nature Cooling Breaking

Page 7: White Carborundum

First Crushing

• Jaw Crusher

Page 8: White Carborundum

Fine Crushing

• Twin Roller

Page 9: White Carborundum

Fine Crushing

• Ball Mill

Page 10: White Carborundum

Sieving

Screening equipment: Coarse Fraction, magnetic seperation, sieving the needed size

Page 11: White Carborundum

Micropowder

Micro Size: F230-F1200, P240-P2500, JIS240-JIS8000, W63-W5

Method: White fused aluminum oxide fines→ball mill→air segment→acid-alkali

washing→water washing→select the particle size( water effusion)→ stoving

→loosen→finshed micopowder

Page 12: White Carborundum

Water Effusion

Page 13: White Carborundum

Introduction of method on selecting micropowder

• Principle of water effusion:Hydraulic impulse